Thursday, August 20, 2009
















NEXT WAS SEALING THE OUTSIDE WOOD. I KNEW LUAN EVEN PAINTED WOULDN'T HOLDUP TO LONG SO DECIDED TO FIBERGLASS OUTSIDE. FIRST SEALER/BONDING COAT. USED POLYESTER RESIN AND ACETONE MIXTURE TO SATURATE WOOD. ONCE TACKY. LAID 6 OZ FIBERGLASS. LAID ANOTHER COAT OF RESIN. APPLIED FINAL COAT RESIN. WASNT TO BAD. LIVED AND WORKED ON MY CRUISING SAILBOATS IN THE PAST. BEING A SURFER DOESN'T HURT EITHER. THAT IS WHY I FINALLY WENT WITH POLYESTER RESIN INSTEAD OF EPOXY.